The best results are achieved by applying the product at room temperature. Room temperature and the temperature of the product should be the same.
- Shake before using for 2 minutes and try it on a cardboard.
- During lacquering hold aerosol with 25÷30 cm of distance from the surface.
- Apply 2 or 3 single layers with an interval of 5 – 10 minutes. Shake aerosol before applying each layer.
- Clean the spray nozzle after use! – Hold the can with the valve pointing downward, press the button emptying the content for about 5 seconds.
Caution: For safety reasons always follow the information provided in the Material Safety Data Sheet.
Can be covered with any varnish*.
Tech data
| Color |
black |
| Gloss grade |
mat |
| Efficiency |
approx. 1.75 m2 dry film 100 μm |
Substrates
Product has very good adhesio to various substrates. It can be applied over:
- Polyester laminates
- Polyester putties
- Epoxy primers
- 2K Acrylic primers
- Steel, galvanized steel and stainless steel
- Aluminium Wash primer
- Plastic
Drying time at 20°C: 2 – 3 hours
* Compatibility test is recommended.
**Drying time depends on air temperature, humidity and thickness of the layer
Caution
To maintain safety, always follow the instructions given in the MSDS for the products.
 |
VOC for mixture = 578g/L |